Processing Properties Metric English Comments
Clamp Pressure 13.8 - 27.6 MPa
2000 - 4000 psi
Calsak CS-72 General Purpose ABS Resin
Product Characteristics:High Impact, High GlossInjection molding grade
Clamp Pressure 13.8 - 27.6 MPa
2000 - 4000 psi
Calsak CS-72L General Purpose ABS Resin
Product Characteristics:High Impact, High GlossInjection molding grade