Annealing Temperature 900.0 °C

@Time 7200 sec
1652 °F

@Time 2.00 hour
Optimum magnetic properties; Then cool to 930°F at a rate of 120°F per hour
Schmolz + Bickenbach 430FR Stainless Steel Bar