Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 1150 - 1200 °C @Thickness >=2.00 mm |
2100 - 2190 °F @Thickness >=0.0787 in |
Solution Annealing, quench with water |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |