Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Annealing Temperature 750.0 - 799 °C
1382 - 1470 °F
Soft; Cooling: Furnace 20°F/hour to 1200°F/ Then air cool; < 230 HB
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel
Description: Thermodur® 2343 is a single melt Extra Fine Structure (EFS) hot work die steel and Supplied in the annealed conditionCharacteristics: Good toughness; Moderate high-temperature strength..