Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 399 - 427 °C | 750 - 800 °F | Soft; Cooling: Furnace; <230 HB |
Schmolz + Bickenbach Thermodur® 2999 Hot Work Die Steel Description: Maximum high-temperature strength, good high-temperature wear resistance, excellent thermal shock resistance and thermal conductivity across the entire range of service temperatures App.. |