Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 343 °C | 650 °F | Stress-relief; Cooling: Furnace |
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |