Polymer Property : Annealing Temperature = 1100 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Annealing Temperature 1100 - 1150 °C
2010 - 2100 °F
Solution Annealing
Outokumpu 353MA® High Temperature Austenitic Stainless Steel
Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but..