Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 17.0 Month | 17.0 Month | |
Dow Corning SE 1885 KIT Two-part, clear, 1:1, addition cure, low temperature cure, low temperature capable, low viscosity.Information provided by Dow Corning |
|||
Shelf Life | 17.0 Month | 17.0 Month | |
Dow Corning SE 1886 KIT Two-part, clear, 1:1, addition cure, low viscosity, good working time.Information provided by Dow Corning |
|||
Shelf Life | 17.0 Month | 17.0 Month | |
Dow Corning Z-6224 SILANE Dow Corning® Z-6224 Silane contains vinylbenzyl and amine organic groups and methoxysilyl inorganic reactivity. The product is supplied in methanol. It is the neutralized (low chloride) version of .. |