Processing Properties | Metric | English | Comments |
---|---|---|---|
Roll Temperature | 130 - 150 °C | 266 - 302 °F | Hotmelt Coating Multi Roller |
EMS-Griltech Griltex® D 1582E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |