Processing Properties Metric English Comments
Roll Temperature 25.0 °C
77.0 °F
Chill, Cast Film Extrusion
Braskem CN8092 EVA Molding Copolymer
CN8092 is an Ethylene-Vinyl Acetate copolymer (EVA) which has a molecular structure that provides easy processing, adhesion, resilience, low hardness, good moisture, and gas barrier properties. It i..