Processing Properties | Metric | English | Comments |
---|---|---|---|
Recrystallization Temperature | 2500 °C | 4530 °F | Deformation level - 99.99% |
Plansee WL10 Lanthanum Oxide-doped Tungsten Tungsten alloy suitable for use as ion sources, lamp electrodes and welding electrodes.Characteristics (compared to pure tungsten):Improved creep resistanceHigher recrystallization temperatureMachin.. |