Processing Properties | Metric | English | Comments |
---|---|---|---|
Recrystallization Temperature | 1500 °C | 2730 °F | Deformation level - 90% |
Plansee WL10 Lanthanum Oxide-doped Tungsten Tungsten alloy suitable for use as ion sources, lamp electrodes and welding electrodes.Characteristics (compared to pure tungsten):Improved creep resistanceHigher recrystallization temperatureMachin.. |