Processing Properties | Metric | English | Comments |
---|---|---|---|
Recrystallization Temperature | 1350 °C | 2460 °F | Deformation level - 99.99% |
Plansee MY Molybdenum-Yttrium-Cerium Oxide Characteristics:Greater resistance to oxidation than pure MoAdheres well to quartz glassEasily weldableApplications:Conductive ESS ribbonsCoating technology - evaporation boatsInformation provided b.. |