Processing Properties | Metric | English | Comments |
---|---|---|---|
Recrystallization Temperature | 900 - 1300 °C | 1650 - 2370 °F | |
ATI Wah Chang Niobium Niobium is a soft, ductile metal which can be cold worked over 90 percent before annealing becomes necessary. In appearance, the metal is somewhat similar to stainless steel. The density of 8.57 gm/.. |