Processing Properties | Metric | English | Comments |
---|---|---|---|
Recrystallization Temperature | 1200 °C | 2190 °F | Deformation level - 90% |
Plansee MoILQ Molybdenum Incandescent Light Quality Characteristics:Recrystallization temperature higher than pure MoFiner grain structure than pure MoApplications: This grade was developed for use in the lighting industry. It is more easily formed.. |
|||
Recrystallization Temperature | 1200 °C | 2190 °F | Deformation level - 90% |
Plansee MW30 Molybdenum-Tungsten Characteristics:Improved high temperature properties when compared to pure tungstenImproved corrosion resistance compared to pure tungstenEnhanced etchabilityApplications:Manufacture of ZincGlass In.. |