Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 5.0000 min | 0.083333 hour | Initial Set |
3M Scotchkote™ PR 504 Urethane Pipe Repair Scotchkote Urethane Pipe Repair PR 504 is a special fast curing moisture activated repair bandage for repair bandage for repairs to leaking pipes.Product Features:Easy to apply, requiring no special.. |