Processing Properties Metric English Comments
Cure Time 19.8 - 40.2 min

@Temperature -65.0 - 450 °C
0.330 - 0.670 hour

@Temperature -85.0 - 842 °F
Handling
Palm Labs Adhesives TURBO-LOCK SERIES 13-OR Anaerobic Thread Locking Compound
TURBO-LOCK 13-OR SERIES is a RED, high temperature, high strength, permanent, oil resistant, anaerobic thread-locking compound. It is highly resistance to heat, vibrations, water, gases, oils, hydro..