Processing Properties Metric English Comments
Cure Time 270 min
4.50 hour
Full Cure
3M Scotchkote™ 175UC Epoxy Coating
Scotchkote Epoxy Coating 175UC has been specifically developed as a 100% solidsProduct Features:Combines good application characteristics with excellent corrosion protection and ultimate chemical re..