Polymer Property : Cure Time = 3600 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 3600 min
60.0 hour
Tack-Free Time
3M AC-236 Class C-20 Aerospace Sealant
3M Aerospace Sealant AC-236 Class C are two-component, manganese dioxide cured, liquid polysulfide polymer systems providing excellent fuel tank and fuselage seals. They have outstanding resistance ..