Polymer Property : Cure Time = 30.0 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 1440 - 1800 min

@Temperature 24.0 °C
24.0 - 30.0 hour

@Temperature 75.2 °F
BCC Products BC 7062-2H Epoxy Casting
BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi..