Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 210 min | 3.50 hour | Fixture time |
ITW Devcon Epoxy Plusâ„¢ 25 Grey Information provided by ITW Devcon |
|||
Cure Time | 210 min | 3.50 hour | Hard Dry |
3M Scotchkote™ PR 415 Epoxy Concrete Repair Scotchkote Epoxy Concrete Repair PR 415 has been specifically developed as a three component 100% solids self priming concrete repair system.Product Features:Combines good application characteristic.. |
|||
Cure Time | 210 - 240 min @Temperature 24.0 °C |
3.50 - 4.00 hour @Temperature 75.2 °F |
demold time |
BCC Products SLO-KAST BC 8009 Urethane Casting Slo-Kast is a low viscosity, medium setting, easy to use casting material. This polyurethane system features extremely low shrinkage when properly cured. Unlike Kwik-Kast, BC 8009 offers the user lo.. |
|||
Cure Time | 210 min @Temperature 93.0 °C |
3.50 hour @Temperature 199 °F |
|
Henkel Hysol EA 9390 Paste Adhesive System Low viscosity system for high temperature wet lay-up composite repair. Qualified to BMS 8-301.Applications: Structural Bonding Low Viscosity Wet Lay-Up Composite Bonding |