Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 1260 min | 21.0 hour | |
3M AC-665 Class C-24 Aerospace Sealant 3M Aerospace Sealant AC-665 Class C are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |