Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 20200 min | 336 hour | Full Cure |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |
|||
Cure Time | 20200 min | 336 hour | |
Lord Adhesives Aeroglaze® A276 Reflective Polyurethane Aeroglaze® A276 reflective polyurethane gives a hard, flexible, colorfast, non-chalking surface that is resistant to most acids, alkaline detergents, lubricants, and chemicals.All information provi.. |