Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 12.0 - 14.0 min | 0.200 - 0.233 hour | Working time |
ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive II, Grey / Beads Information provided by ITW Devcon |
|||
Cure Time | 6.00 - 14.0 min | 0.100 - 0.233 hour | t`90; ASTM D2084 |
ExxonMobil Exxon™ 2222 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product for is white to light amber bales.Information provided by ExxonMobil Chemical |
|||
Cure Time | 6.00 - 14.0 min | 0.100 - 0.233 hour | t`90; ASTM D2084 |
ExxonMobil Exxon™ 2235 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is white to light amber bales.Information provided by ExxonMobil Chemical |
|||
Cure Time | 6.00 - 14.0 min | 0.100 - 0.233 hour | t`90; ASTM D2084 |
ExxonMobil Exxon™ 2255 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene.The product form is white to light amber bales.Information provided by ExxonMobil Chemical |
|||
Cure Time | 8.00 - 14.0 min | 0.133 - 0.233 hour | t`90; ASTM D2084 |
ExxonMobil Exxon™ 6222 Brominated Star-Branched Butyl Exxon SB Bromobutyl is a brominated copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical |