Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 5.00 - 11.0 min | 0.0833 - 0.183 hour | t`50; ASTM D2084 |
ExxonMobil Exxon™ 2222 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product for is white to light amber bales.Information provided by ExxonMobil Chemical |