Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 1.60 - 960 min @Temperature 68.3 - 204 °C |
0.0267 - 16.0 hour @Temperature 155 - 400 °F |
Average value: 31.0 min Grade Count:407 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |