Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 24.0 min @Temperature 154 °C |
0.400 hour @Temperature 310 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Hi-Sil 243 LD Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 24.0 min @Temperature 154 °C |
0.400 hour @Temperature 310 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Hi-Sil 243 LD Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |