Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.0667 - 0.100 min | 0.00111 - 0.00167 hour | Plastic set time |
Lord Adhesives 7700 Fast Setting, High Viscosity, Impact Resistant. Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.0667 - 0.100 min | 0.00111 - 0.00167 hour | Rubber set time |
Lord Adhesives 7700 Fast Setting, High Viscosity, Impact Resistant. Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |