Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 4.50 - 10.5 min | 0.0750 - 0.175 hour | t`50; ASTM D2084 |
ExxonMobil Exxon™ 2235 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is white to light amber bales.Information provided by ExxonMobil Chemical |
|||
Cure Time | 4.50 - 10.5 min | 0.0750 - 0.175 hour | t`50; ASTM D2084 |
ExxonMobil Exxon™ 2255 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene.The product form is white to light amber bales.Information provided by ExxonMobil Chemical |