Polymer Property : Cure Time = 0.016666 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 0.016666 - 0.500 min
0.00027777 - 0.00833 hour
3M Scotch-Weld™ CA7 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to metals, plastics, and rubbers.Information provided by 3..