Polymer Property : Back Pressure = 160 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 0.700 - 1.10 MPa
102 - 160 psi
Hydraulic backpressure
Perstorp Compounds 136 Urea-Formaldehyde w/ cellulose filler
A UF-based injection grade designed for hidden parts like sockets, circuit breakers, clamps, switches.Information provided by Perstorp Compounds Inc.