Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 5 - 7 hour | 5 - 7 hour | Use immediately after drying. |
Tipco Tipwood® 50 EX 50EX Description: Tipwood® is a Wood-Fiber Reinforced, Heat Stabilized Polypropylene Compound specially developed by Tipco for Automobile Interiors and Appliance Fascia Applications.Features: Environmen.. |