Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 10 - 12 hour | 10 - 12 hour | for PET systems |
Süd-Chemie Nanofil® 2 Polymer Additive Application:PETFilmBottlesImproves: Barrier |
|||
Dry Time | 10 - 12 hour | 10 - 12 hour | for PET systems |
Süd-Chemie Nanofil® SE 3000 Flame Retardant Application:PE/EVA; PP Cable formulationAutomotiveFilmTechnical PartsImproves: Scratch Resistance, Barrier, Mechanical Properties, Melt Viscosity, Flame Retardancy |