Polymer Property : Dry Time = 0.333 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dry Time >= 0.333 hour
>= 0.333 hour
Hexcel® Redux® 108 Surface Pretreatment Protection Solution
The Redux 100 series is a range of resin solutions used for protecting light alloy surfaces that have been pretreated for bonding but must be stored temporarily before bonding is completed.A thin co..
Dry Time >= 0.333 hour
>= 0.333 hour
Hexcel® Redux® 112 Surface Pretreatment Protection Solution
The Redux 100 series is a range of resin solutions used for protecting light alloy surfaces that have been pretreated for bonding but must be stored temporarily before bonding is completed.A thin co..
Dry Time 0.333 hour
0.333 hour
50% RH
3M Scotchcast™ 5400 Electrical Powder Resin
3M Scotchcast Electrical Resin 5400 has been specially developed for continuous coating process. It is well suited for applications where flexibility and resistance to cracking due to heat shock or ..