Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 0.33 hour | 0.33 hour | |
Taiwan PU Corporation TPUCO Polyurethane Sealing Resin PU sealing resin is a waterproof, insulated protective film made of quality PU resin. It is used in the prevention of humidity, germs, collision, corrosion, parts loosening, and rusting, and as ins.. |