Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 0.167 - 0.250 hour | 0.167 - 0.250 hour | |
Hexcel® Redux® 101 Surface Pretreatment Protection Solution The Redux 100 series is a range of resin solutions used for protecting light alloy surfaces that have been pretreated for bonding but must be stored temporarily before bonding is completed.A thin co.. |