Processing Properties Metric English Comments
Drying Temperature 149 - 270 °C
300 - 518 °F
Average value: 178 °C Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a..