Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 48.9 - 54.4 °C | 120 - 130 °F | |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Drying Temperature | 48.9 - 54.4 °C | 120 - 130 °F | |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Drying Temperature | 48.9 - 65.6 °C | 120 - 150 °F | |
PolyOne Lubri-Tech™ SY-000/10T-2S Natural Polystyrene (PS), PTFE Lubricated
(discontinued **) Description/Features:High ImpactPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 48.9 - 65.6 °C | 120 - 150 °F | Usually not required |
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Drying Temperature | 48.9 - 65.6 °C | 120 - 150 °F | Usually not required |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Drying Temperature | 48.9 - 65.6 °C | 120 - 150 °F | Usually not required |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Drying Temperature | 48.9 - 65.6 °C | 120 - 150 °F | Usually not required |
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add.. |
|||
Drying Temperature | 48.9 °C @Time 7200 - 21600 sec |
120 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 124789 B Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 89% Renewable Resource Content Not optically transparent. Thick wall sections can be hazy. For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Drying Temperature | 48.9 °C @Time 7200 - 21600 sec |
120 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 124789 C Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 84% Renewable Resource Content Not optically transparent. Thick wall sections can be hazy. For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Drying Temperature | 48.9 °C @Time 7200 - 21600 sec |
120 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 124789 D Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 79%Renewable Resource Content Not optically transparent. Thick wall sections can be hazy. For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Drying Temperature | 48.9 °C @Time 7200 - 21600 sec |
120 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 126211 Z Bio-Based Polylactic Acid (PLA); FDA Compliant Ingredients - Impact Modified - Transparent - 89% Renewable Resource Content Not optically transparent. Thick wall sections can be hazy. For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Drying Temperature | 48.9 °C @Time 7200 - 21600 sec |
120 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 126217 Z Bio-Based Polylactic Acid (PLA); Impact Modified - FDA Compliant Ingredients - 79% Renewable Resource Content For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Drying Temperature | 48.9 °C @Time 7200 - 21600 sec |
120 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 126218 A Bio-Based Polylactic Acid (PLA); Impact Modified - 94% Renewable Resource Content For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Drying Temperature | 48.9 °C @Time 7200 - 21600 sec |
120 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 126218 B Bio-Based Polylactic Acid (PLA); Impact Modified - 89% Renewable Resource Content For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Drying Temperature | 48.9 °C @Time 7200 - 21600 sec |
120 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 126218 C Bio-Based Polylactic Acid (PLA); Impact Modified - 84% Renewable Resource Content For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Drying Temperature | 48.9 °C @Time 7200 - 21600 sec |
120 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 126218 D Bio-Based Polylactic Acid (PLA); Impact Modified - 79% Renewable Resource Content For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Drying Temperature | 48.9 °C @Time 7200 - 21600 sec |
120 °F @Time 2.00 - 6.00 hour |
|
RTP Company RTP 2099 X 124789 A Bio-Based Polylactic Acid (PLA); Impact Modified - Transparent - 94% Renewable Resource Content Not optically transparent. Thick wall sections can be hazy. For detailed processing information, see the PLA Molding Guide on the RTP Company website. |