Processing Properties Metric English Comments
Drying Temperature 107 °C

@Time 14400 - 21600 sec
225 °F

@Time 4.00 - 6.00 hour
RTP Company RTP 4000 A-1230 L Polyphthalamide (PPA), Mineral - Lubricated
Drying Temperature 107 °C
225 °F
RTP Company RTP 4000 A-1240 L Polyphthalamide (PPA), Mineral
Drying Temperature 107 °C
225 °F
RTP Company RTP 4000 AF-1115 V0 Polyphthalamide (PPA), Glass Fiber - Mineral - Flame Retardant
Drying Temperature 107 °C
225 °F
RTP Company RTP 4000 AF-1550 V0 Polyphthalamide (PPA), Glass Fiber - Mineral - Flame Retardant
Drying Temperature 107 °C
225 °F
RTP Company RTP 4000 AR 15 TFE 15 Polyphthalamide (PPA), Aramid Fiber - PTFE Lubricated
Drying Temperature 107 °C
225 °F
RTP Company RTP 4000 MG 50 Polyphthalamide (PPA), Milled Glass
Drying Temperature 107 °C
225 °F
RTP Company RTP 4000 TFE 10 Polyphthalamide (PPA), PTFE Lubricated
Drying Temperature 107 °C
225 °F
RTP Company RTP 4003 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Drying Temperature 107 °C
225 °F
RTP Company RTP 4003 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Drying Temperature 107 °C
225 °F
RTP Company RTP 4004 FR A HS Polyphthalamide (PPA), Glass Fiber - Flame Retardant - Heat Stabilized
Drying Temperature 107 °C

@Time 14400 - 21600 sec
225 °F

@Time 4.00 - 6.00 hour
RTP Company RTP 4005 TFE 10 Polyphthalamide (PPA), Glass Fiber - PTFE Lubricated
Drying Temperature 107 °C
225 °F
RTP Company RTP 4007 TFE 10 Polyphthalamide (PPA), Glass Fiber - PTFE Lubricated
Drying Temperature 107 °C
225 °F
RTP Company RTP 4008 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Drying Temperature 107 °C
225 °F
RTP Company RTP 4083 A (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber
Drying Temperature 107 °C
225 °F
RTP Company RTP 4085 A TFE 15 (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - PTFE Lubricated
Drying Temperature 107 °C
225 °F
RTP Company RTP 4085 SI 2 Polyphthalamide (PPA), Carbon Fiber - Silicone Lubricated
Drying Temperature 107 °C
225 °F
RTP Company RTP 4087 A FR (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - Flame Retardant
Drying Temperature 107 °C
225 °F
RTP Company RTP 4087 TFE 15 Polyphthalamide (PPA), Carbon Fiber - PTFE Lubricated
Drying Temperature 107 °C

@Time 14400 - 21600 sec
225 °F

@Time 4.00 - 6.00 hour
RTP Company RTP 4099 X 113516 A Polyphthalamide (PPA) Glass Fiber - Flame Retardant - Halogen Free
Drying Temperature 107 - 113 °C
225 - 235 °F
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend
Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc.
Drying Temperature 107 °C

@Time 21600 sec
225 °F

@Time 6.00 hour
RTP Company RTP 1200 S-55D Ester-based Thermoplastic Polyurethane Elastomer
Drying Temperature 107 °C

@Time 14400 - 21600 sec
225 °F

@Time 4.00 - 6.00 hour
RTP Company RTP 2300 A Rigid Thermoplastic Polyurethane (RTPU), Base Resin
Drying Temperature 107 °C
225 °F
RTP Company RTP 2307 A Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber
Drying Temperature 107 °C

@Time 14400 - 21600 sec
225 °F

@Time 4.00 - 6.00 hour
RTP Company RTP 2505 A TFE 15 Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber - PTFE Lubricated
Drying Temperature 107 °C

@Time 21600 sec
225 °F

@Time 6.00 hour
RTP Company RTP 1200 T-70A UV Ether-based Thermoplastic Polyurethane Elastomer (; UV Stabilized
Drying Temperature 107 - 140 °C
225 - 284 °F
Average value: 114 °C Grade Count:5
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..
Drying Temperature 107 °C

@Time 14400 - 21600 sec
225 °F

@Time 4.00 - 6.00 hour
RTP Company RTP 4005 TFE 13 SI 2 Polyphthalamide (PPA) Glass Fiber - PTFE Lubricated - Silicone Lubricated
Drying Temperature 107 °C
225 °F
RTP Company RTP 4005.3 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Drying Temperature 107 °C

@Time 14400 - 21600 sec
225 °F

@Time 4.00 - 6.00 hour
RTP Company RTP 4082 AR 15 Polyphthalamide (PPA); Carbon & Aramid Fiber Reinforced - Wear Resistant
Drying Temperature 107 °C
225 °F