Processing Properties Metric English Comments
Rear Barrel Temperature 277 - 291 °C
530 - 555 °F
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 277 - 291 °C
530 - 555 °F
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 277 - 291 °C
530 - 555 °F
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 277 - 291 °C
530 - 555 °F
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).