Processing Properties Metric English Comments
Rear Barrel Temperature 154 - 193 °C
309 - 379 °F
PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE)
Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - ..
Rear Barrel Temperature 154 - 177 °C
309 - 351 °F
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol..