Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 116 - 149 °C | 241 - 300 °F | |
PolyOne Versaflex™ CL2000X Thermoplastic Elastomer (TPE) Versaflex™ CL2000X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and an extremely soft feel are desired. - Tactile Feel - Ultra-Soft - Water Clar.. |