Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 146 - 185 °C | 295 - 365 °F | |
PolyOne Versaflex™ CL2050 Thermoplastic Elastomer (TPE) Versaflex™ CL2050 is an easy processing compound designed for use in applications where clarity and enhanced heat resistance are required. New Product. Commercial specifications have not been estab.. |