Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 143 - 171 °C | 289 - 340 °F | |
PolyOne Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6703-0001 is an easy processing compound designed for use in injection molding applications where extremely soft feel properties are desired. - Excellent Colorability - Good Ozone and UV.. |