Polymer Property : Mold Temperature = 340 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 171 - 193 °C
340 - 380 °F
Bulk Molding Compounds BMC 324 Automotive Grade Molding Compound
BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-co..