Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 71.1 - 132 °C | 160 - 270 °F | Average value: 103 °C Grade Count:7 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |