Polymer Property : Mold Temperature = 221 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 204 - 221 °C
399 - 430 °F
Blow Molding
PolyOne Geon™ Vinyl Packaging 2797 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Mold Temperature 204 - 221 °C
399 - 430 °F
Blow Molding
PolyOne Geon™ Vinyl Packaging 2798 Polyvinyl Chloride, Rigid (PVC, Rigid)
Premium chemical resistant Compound for Packaging.Information provided by PolyOne