Nozzle Temperature 379 °C
715 °F
Oxford Polymers PEEK 20GF-Natural PEEK, 20% Glass Fiber Reinforced
Product Description: Glass Fiber (20% Reinforced), PEEK, Polyetheretherketone injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass fiber Special Chara..