Polymer Property : Nozzle Temperature = 425 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 360 - 425 °C
680 - 797 °F
Average value: 387 °C Grade Count:6
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Nozzle Temperature 360 - 425 °C
680 - 797 °F
Average value: 393 °C Grade Count:13
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..