Polymer Property : Nozzle Temperature = 340 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 171 - 210 °C
340 - 410 °F
PolyOne Versaflex™ 9545-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9545-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Nozzle Temperature 171 - 210 °C
340 - 410 °F
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Nozzle Temperature 171 - 210 °C
340 - 410 °F
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE)
Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Nozzle Temperature 171 - 210 °C
340 - 410 °F
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Nozzle Temperature 171 - 210 °C
340 - 410 °F
PolyOne Versalloy™ HC 9210-45N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-45N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgic..
Nozzle Temperature 171 - 210 °C
340 - 410 °F
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod..
Nozzle Temperature 171 - 210 °C
340 - 410 °F
PolyOne Versalloy™ HC 9210-70N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-70N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items and soft-touch overmolding for surgical grips. Product ex..
Nozzle Temperature 171 - 210 °C
340 - 410 °F
PolyOne Versalloy™ XL 9045-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9045-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
Nozzle Temperature 171 - 210 °C
340 - 410 °F
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-100 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-110 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-120 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-130 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-140 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-145 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-150 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-155 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-160 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-205 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-210 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-215 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-220 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-225 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-235 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-300 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Moisture can..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-305 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Moisture can..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-310 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Moisture can..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-315 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Moisture can..
Nozzle Temperature 171 - 193 °C
340 - 380 °F
Teknor Apex Medalist® MD-320 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Moisture can..
Nozzle Temperature 171 - 206 °C
340 - 402 °F
Tempia Polylactic acid (PLA) Resin
A bio-degradable plastic, Polylactic acid (PLA) is made from corn. Products produced are compostable within 45 – 120 days. The degradation process of the item is temperature, humidity and thicknes..